CNT aerogel interlayer cuts carbon-composite heat-up time by 57%
A CNT/Fe3O4/PA6 aerogel interlayer lifted initial heating 94.6%, cut time to the joining temperature 57% and raised joint strength 30.8% in KIMS trials.