Heat and humidity cut PLA impact strength by 80% over six months
IMDEA Materials researchers found that PLA absorbed only 0.3%-0.7% moisture over six months at 40°C, yet impact strength fell about 80%; hexagonal boron nitride retained 86% toughness.

SPECIFICATION
- 1
Aging ran for six months at 40°C and 75% relative humidity.
- 2
PLA absorbed only 0.3%-0.7% moisture by weight.
- 3
Neat PLA and NC-filled PLA lost about 80% of impact strength.
- 4
The hBN composite retained about 86% of its original impact toughness.
- 5
The study appeared in Polymer Degradation and Stability in 2026.
Neat PLA and PLA reinforced with organomodified nanoclay (NC) lost about 80% of their impact strength after six months at 40°C (104°F) and 75% relative humidity, IMDEA Materials Institute researchers report.
That result came from a study published in Polymer Degradation and Stability. The team examined how heat and humidity change PLA reinforced with two-dimensional (2D) nanomaterials. The work links moisture-driven damage to specific chemical processes and tests one filler that better protected those properties.
Demand for sustainable alternatives to conventional plastics continues to grow. PLA, a biodegradable thermoplastic used in packaging and consumer products, fits that demand. Its long-term reliability during humid storage and service remains the critical challenge.
A six-month test filled the evidence gap
Earlier studies often used short-term water immersion. Petronela Chovancová said: “Previous studies have often focused on short-term water immersion tests, but these conditions do not always accurately reflect the variety of environments materials experience during storage or service.”
The IMDEA Materials team used hygrothermal aging (the combined effects of heat and humidity) under conditions intended to represent real storage and service environments. The comparison covered neat PLA and three composite series. Each composite contained one two-dimensional nanofiller.
- Aging condition: 40°C (104°F) and 75% relative humidity.
- Exposure period: Six months.
- Nanofillers: Organomodified nanoclay (NC), graphene nanoplatelets (GNP) and hexagonal boron nitride (hBN).
The study placed neat PLA alongside composites containing one of three nanofillers. Its aim was to measure how each nanomaterial influenced PLA degradation during prolonged humidity exposure. The researchers were Petronela Chovancová, Miguel Hernández del Valle, Dr. Maciej Haranczyk and Dr. Juan Pedro Fernández Blázquez.
Low moisture uptake still meant severe damage
After six months, moisture uptake remained between just 0.3% and 0.7% by weight. The small gain did not prevent mechanical and rheological deterioration.
Neat PLA and PLA reinforced with NC lost around 80% of impact strength, a severe loss in impact resistance. Rheological analysis tracked polymer flow when molten and also found a dramatic reduction in melt viscosity. That drop indicated extensive degradation of the polymer structure.
The result separates water absorption from material durability. Even limited exposure to moisture can carry significant consequences for a biodegradable polymer’s long-term performance.
Hexagonal boron nitride gave the strongest protection
Among the three nanomaterials, hexagonal boron nitride (hBN) delivered the best overall performance. The hBN-reinforced nanocomposite retained approximately 86% of its original impact toughness after six months of aging. It significantly outperformed the other formulations.
Thermal analysis showed that the filler helped maintain stable crystallization throughout the conditioning period. It also helped preserve PLA’s rheological properties during aging.
The findings identify hBN as a promising nanofiller for PLA-based materials exposed to prolonged humidity. They may guide the development of biodegradable materials for applications where humidity exposure matters.
What does this change for PLA product teams?
“We found that short-term exposure to liquid water primarily causes plasticization, a reversible process in which absorbed water increases polymer chain mobility,” Chovancová said. “This effect can temporarily improve toughness and flexibility, even while initial degradation processes begin.”
“Long-term exposure to humidity, however, follows a different path. Over time, moisture promotes hydrolytic chain scission, progressively breaking down polymer chains within the material. This irreversible chemical degradation ultimately results in embrittlement, reduced toughness and a collapse in melt viscosity,” she concluded.
Hydrolytic chain scission is the water-driven breaking of polymer chains. The distinction matters because temporary softening is not permanent damage. PLA can gain flexibility briefly while its long-term toughness and flow behaviour deteriorate.
For packaging and consumer-product teams, short immersion tests alone cannot establish PLA’s long-term durability in humid service. Low moisture uptake is not a safe proxy for durability. Among the three fillers tested, hBN gave the strongest overall performance, including 86% impact-toughness retention. The findings can guide material development where long-term humidity exposure matters.
The paper, Long-term hygrothermal degradation of PLA 2D nanocomposites: Decoupling plasticisation from chemical degradation, appeared in Polymer Degradation and Stability in 2026. Its DOI is 10.1016/j.polymdegradstab.2026.112481.